National Association of Testing Authorities, Australia
Scope of Accreditation
Adbri Cement
Scope of Accreditation
ISO/IEC 17025 (2017)
Infrastructure and Asset Integrity
Service | Product | Determinant | Technique | Procedure | Limitations |
---|---|---|---|---|---|
Evaluation of geotechnical and civil construction material - Aggregate contaminants | Aggregates | Clay and fine silt; Organic impurities | Colour test; Settling | AS 1141.33, AS 1141.34 | |
Evaluation of geotechnical and civil construction material - Aggregate properties | Aggregates | Shape | Elongation; Flakiness; Proportional calliper | AS 1141.14, AS 1141.15; DPTI (SA) Method TP240, DPTI (SA) Method TP241 | |
Particle size distribution | Sieve analysis; Sieve analysis of material finer than 75 µm | AS 1141.11.1, AS 1141.12 | |||
Bulk density | Compacted; Uncompacted | AS 1141.4 | |||
Particle density of coarse aggregate; Particle density of fine aggregate | Weighing-in-water | AS 1141.5, AS 1141.6.1 | |||
Moisture content | Drying oven | AS 1289.2.1.1 | |||
Evaluation of geotechnical and civil construction material - Concrete, grout and mortar consistence in situ | Concrete, grout and mortar | Slump flow | Cone | AS 1012.3.1 ASTM C1611 | |
Evaluation of geotechnical and civil construction material - Concrete, grout and mortar permeability | Concrete, grout and mortar | Permeability; Sorptivity | Volume change with water absorption - Permeable voids | AS 1012.21 | |
Evaluation of geotechnical and civil construction material - Concrete, grout and mortar properties | Concrete, grout and mortar | Mass per unit volume - Fresh concrete | In situ measurement using fixed volume measure | AS 1012.5 | |
Bleeding | In situ analysis - Freshly mixed concrete | AS 1012.6 | |||
Flexural strength | Modulus of rupture | AS 1012.11 | |||
Mass per unit volume - Hardened concrete | Dimensions; Water displacement | AS 1012.12.1 AS 1012.12.2 | |||
Compressive strength | Core; Cube; Cylinder | AS 1012.9 AS 1012.14 | |||
Air content of freshly mixed concrete | Reduced air pressure | AS 1012.4.2 | |||
Uniformity of mixing | Not applicable | AS 1379 Appendix A | |||
Evaluation of geotechnical and civil construction material - Concrete, grout and mortar shrinkage | Concrete, grout and mortar | Drying shrinkage specimen measurement | Not applicable | AS 1012.13 | |
Evaluation of geotechnical and civil construction material - Concrete, grout and mortar specimen manufacture and curing | Concrete, grout and mortar | Specimen conditioning; Specimen manufacture; Specimen manufacture and curing | Curing grout and mortar cube specimens in the laboratory; In situ manufacture and curing of cylindrical specimens; In situ manufacture and curing of drying shrinkage specimens; In situ manufacture and curing of flexural strength specimens; In situ manufacture and curing of grout and mortar cubes; Manufacture and curing of cylindrical specimens in the laboratory; Manufacture and curing of drying shrinkage specimens in the laboratory; Manufacture and curing of fibre reinforced specimens in the field; Manufacture and curing of grout and mortar cubes in the laboratory; Mixing concrete in the laboratory; Wet conditioning of hardened concrete core specimens | AS 1012.2; AS 1012.8.1 AS 1012.8.2, AS 1012.8.3, AS 1012.8.4, AS 1012.14RMS (NSW) Method T304 TfNSW TS 02800.05 | |
Sample collection | Aggregates | Not applicable | Aggregate from a stockpile | AS 1141.3.1 | |
Concrete, grout and mortar | Not applicable | Fresh concrete from a mixer | AS 1012.1 |
ISO/IEC 17025 (2017)
Materials
Service | Product | Determinant | Technique | Procedure | Limitations |
---|---|---|---|---|---|
Analysis of cements and cementitious materials - Composition | Cement products | Insoluble residue | Classical - Dry ingredients | AS 2350.2 | |
Lime - Free | Classical - Dry ingredients; Classical - Hydrated material | ASTM C114/30 | |||
Aluminium oxide; Calcium oxide; Ferric oxide; Magnesium oxide; Manganese monoxide; Phosphorus pentoxide; Potassium oxide; Silicon dioxide; Sodium oxide; Sulfur trioxide (sulfuric anhydride); Titanium oxide | Combustion; X-ray fluorescence (XRF) - Dry ingredients; X-ray fluorescence (XRF) - Hydrated material | AS 2350.2, AS 4489.5.1, ASTM C114 and in-house BH-TM-0507 | |||
Chloride | Classical - Dry ingredients | AS 3583.13 | |||
Lime - Available | Classical - Dry ingredients | AS 4489.6.1 | |||
Chloride | X-ray fluorescence (XRF) - Dry ingredients | In-house method BH-TM-0507 | |||
Sulfide | Classical - Dry ingredients; Classical - Hydrated material | AS 3583.8 | |||
Loss on ignition | Gravimetric | AS 2350.2 AS 4489.7.1 | |||
Moisture - Free | Gravimetric | AS 4489.8.1 | |||
Sulfur trioxide (sulfuric anhydride) | Combustion | AS 2350.2 and in-house method BH-TM-0547 | |||
Chloride - Acid soluble; Sulfate - Acid soluble | X-ray fluorescence (XRF) - Hydrated material | AS 1012.20.1 | |||
Cement products; Pozzolanic materials | Calcium oxide; Carbon dioxide (CO2); Sulfur trioxide (sulfuric anhydride) | Combustion | AS 4489.5.1 and in-house method BH-TM-0547 | ||
Pozzolanic materials | Sulfur trioxide (sulfuric anhydride) | Combustion | AS 2350.2 and in-house method BH-TM-0547 | ||
Available alkali | Classical - Dry ingredients; Classical - Hydrated material | AS 3583.12 | |||
Loss on ignition | Gravimetric | AS 3583.3 | |||
Aluminium oxide; Calcium oxide; Ferric oxide; Magnesium oxide; Manganese monoxide; Potassium oxide; Silicon dioxide; Sodium oxide; Sulfur trioxide (sulfuric anhydride); Titanium oxide | X-ray fluorescence (XRF) - Dry ingredients; X-ray fluorescence (XRF) - Hydrated material | AS 2350.2, ASTM C114 and in-house BH-TM-0507 | |||
Sulfide - Total | Classical - Dry ingredients; Classical - Hydrated material | AS 3583.7 | |||
Chloride | Classical - Dry ingredients | AS 3583.13 | |||
Moisture - Free | Gravimetric | AS 3583.2 | |||
Acid soluble residues | Classical - Dry ingredients | AS 3583.14 | |||
Analysis of cements and cementitious materials - Properties | Cement products | Relative density (specific gravity) | Displacement | AS 3583.5 | |
Soundness of limes and limestones; Soundness of portland and blended cement | Cement pat; Le Chatelier | AS/NZS 2350.5; AS 4489.4.1; AS 4489.4.2 | |||
Fineness index | Air permeability | AS/NZS 2350.8 | |||
Temperature rise | AS 2350.7 | ||||
Consistency; Setting time | Cone impression; Normal consistency | AS/NZS 2350.3; AS/NZS 2350.4 | |||
Drying shrinkage; Length change | Length change with exposure to sulfate solution | AS 2350.13; AS 2350.14 | |||
Fineness index | Air permeability | AS/NZS 2350.8 | |||
Slaking properties | Not applicable | AS 4489.3.1 | |||
Cement products; Pozzolanic materials | Compressive strength; Relative strength and water requirement | Not applicable | AS/NZS 2350.11; AS 3583.6 | ||
Sample preparation of portland and blended cement; Sample preparation of pozzolanic materials | Not applicable | AS 2350.12 | |||
Bulk density; Relative density (specific gravity) | Displacement; Fixed volume measure | AS 3583.5; AS 4489.10.1; ASTM C188 | |||
Fineness of lime and limestone | Wet sieving | AS 4489.2.1 | |||
Pozzolanic materials | Relative density (specific gravity) | Displacement | AS 3583.5 | ||
Fineness index | Air permeability | AS/NZS 2350.8 | |||
Analysis of ores and minerals | Dolomite; Limestone | Loss on ignition | Gravimetric | AS 4489.7.1 | |
Chloride | Classical | AS 3583.13 | |||
Aluminium oxide; Calcium oxide; Ferric oxide; Magnesium oxide; Manganese oxide; Phosphorus pentoxide; Potassium oxide; Silicon dioxide; Sodium oxide; Sulfur trioxide (sulfuric anhydride); Titanium oxide | X-ray fluorescence (XRF) | AS 2350.2, ASTM C114 and in-house BH-TM-0507 | |||
Gypsum | Aluminium oxide; Calcium oxide; Ferric oxide; Magnesium oxide; Manganese oxide; Phosphorus pentoxide; Potassium oxide; Silicon dioxide; Sodium oxide; Sulfur trioxide (sulfuric anhydride); Titanium oxide | X-ray fluorescence (XRF) | AS 2350.2, ASTM C114 and in-house BH-TM-0507 | ||
Loss on ignition | Gravimetric | AS 2350.2 | |||
Chloride | Classical | AS 3583.13 | |||
Silica sands | Loss on ignition | Gravimetric | AS 2350.2 | ||
Aluminium oxide; Calcium oxide; Ferric oxide; Magnesium oxide; Manganese oxide; Phosphorus pentoxide; Potassium oxide; Silicon dioxide; Sodium oxide; Sulfur trioxide (sulfuric anhydride); Titanium oxide | X-ray fluorescence (XRF) | AS 2350.2, ASTM C114 and in-house BH-TM-0507 | |||
Analysis of refractories, ceramics and related materials | Clays | Loss on ignition | Classical | AS 2350.2 | |
Aluminium oxide; Calcium oxide; Ferric oxide; Magnesium oxide; Manganese oxide; Phosphorus pentoxide; Potassium oxide; Silicon dioxide; Sodium oxide; Sulfur trioxide (sulfuric anhydride); Titanium oxide | X-ray fluorescence (XRF) | AS 2350.2, ASTM C114 and in-house BH-TM-0507 |
The only data displayed is that deemed relevant and necessary for the clear description of the activities and services covered by the scope of accreditation.
Grey text appearing in a SoA is additional freetext providing further refinement or information on the data in the preceding line entry.
Accreditation No.